Abstract:
A TOTAL OF SIX DIFFERENT ALLOYS - STAINLESS STEEL TYPES 310, 310S, 347, AND 446, AND NICKEL ALLOYS 800 AND 671 - WERE TESTED USING THE SLOW STRAIN- RATE TEST TECHNIQUE IN OXIDIZING/SULFIDIZING AND IN OXIDIZING/SULFIDIZING/ CARBURIZING SIMULATED COAL GASIFICATION ENVIRONMENTS, AND IN HELIUM (AND OTHER INERT ENVIRONMENTS) AT BOTH 450 AND 600 C AT A STRAIN RATE OF 0.000001/S. OF THE SIX ALLOYS, FOUR (TYPES 310 STAINLESS STEEL AND 310S STAINLESS STEEL, NICKEL ALLOY 800, AND NICKEL ALLOY 671) WERE FOUND TO BE SUSCEPTIBLE TO CRACKING AT 600 C BY POSSIBLY DIFFERENT MECHANISMS, HOWEVER, ALL WERE DETECTED BY THE SLOW STRAIN-RATE TECHNIQUE.
| Pages: |
19 |
| Report Date: |
79 |
| Report Number: |
D241611 |
Report Unavailable |
| This title is unavailable from Storming Media. We do not know when it might be available, if at all. We list the report on our site for bibliographic completeness, to help our users know what other work has been performed in this field. Please note that as with all titles on this site, we do not have contact information for any of the authors. Nor can we give any suggestions on how one might obtain this report. |
|
|
|